Live Construction Material Prices
Track cement, steel, sand, bricks, plumbing, electrical, plywood, and paint prices across 10 Indian cities. With monthly trends and city comparison.
Avg Monthly Change (Bengaluru)
+1.6%
Cheapest City
Jaipur
Costliest City
Mumbai
Cement(2 items)
| Material | Bengaluru | vs Last Month |
|---|---|---|
OPC 53 Grade Cement IS 12269:2013 | ₹390 | ▲ 1.3% |
PPC Cement IS 1489:1991 | ₹360 | ▲ 1.4% |
Steel(2 items)
| Material | Bengaluru | vs Last Month |
|---|---|---|
TMT Steel Fe 500D — 8mm IS 1786:2008 | ₹62 | ▲ 1.6% |
TMT Steel Fe 500D — 12mm IS 1786:2008 | ₹58 | ▲ 1.8% |
Sand & Aggregates(3 items)
| Material | Bengaluru | vs Last Month |
|---|---|---|
River Sand (Zone II) IS 383:2016 | ₹3,200 | ▲ 3.2% |
M-Sand (Manufactured Sand) IS 383:2016 | ₹1,800 | ▲ 2.9% |
20mm Coarse Aggregate IS 383:2016 | ₹1,400 | ▲ 1.4% |
Bricks & Blocks(2 items)
| Material | Bengaluru | vs Last Month |
|---|---|---|
Red Clay Bricks (Class A) IS 1077:1992 | ₹8,500 | ▲ 1.2% |
AAC Blocks (600×200×200mm) IS 2185 Part 3 | ₹4,200 | ▲ 1.2% |
Plumbing(1 items)
| Material | Bengaluru | vs Last Month |
|---|---|---|
CPVC Pipe (½ inch / 15mm) IS 15778:2007 | ₹85 | ▲ 1.2% |
Electrical(1 items)
| Material | Bengaluru | vs Last Month |
|---|---|---|
FR Copper Wire 1.5 sq.mm IS 694:2010 | ₹1,850 | ▲ 1.1% |
Wood & Plywood(2 items)
| Material | Bengaluru | vs Last Month |
|---|---|---|
BWP Marine Plywood (18mm) IS 710:2010 | ₹3,200 | ▲ 1.6% |
Laminate Sheet (1mm, Matte) IS 2046 | ₹1,400 | ▲ 1.4% |
Paints(2 items)
| Material | Bengaluru | vs Last Month |
|---|---|---|
Interior Emulsion Paint (Premium) IS 15489 | ₹420 | ▲ 1.2% |
Exterior Emulsion Paint IS 15489 | ₹350 | ▲ 1.4% |
City Comparison — Key Materials
Compare prices of essential materials across all 10 cities at a glance.
| Material | Bengaluru | Mumbai | Delhi NCR | Chennai | Hyderabad | Pune | Kolkata | Ahmedabad | Kochi | Jaipur |
|---|---|---|---|---|---|---|---|---|---|---|
| OPC 53 Grade Cement | ₹390 | ₹410 | ₹380 | ₹375 | ₹370 | ₹400 | ₹385 | ₹375 | ₹395 | ₹365 |
| TMT Steel Fe 500D — 8mm | ₹62 | ₹64 | ₹60 | ₹61 | ₹59 | ₹63 | ₹58 | ₹60 | ₹63 | ₹58 |
| River Sand (Zone II) | ₹3,200 | ₹4,500 | ₹2,800 | ₹3,500 | ₹2,600 | ₹3,800 | ₹2,400 | ₹2,500 | ₹3,000 | ₹2,200 |
| Red Clay Bricks (Class A) | ₹8,500 | ₹10,000 | ₹7,500 | ₹8,000 | ₹7,000 | ₹9,000 | ₹6,500 | ₹7,000 | ₹8,500 | ₹6,500 |
| CPVC Pipe (½ inch / 15mm) | ₹85 | ₹90 | ₹82 | ₹80 | ₹78 | ₹88 | ₹78 | ₹80 | ₹85 | ₹76 |
| BWP Marine Plywood (18mm) | ₹3,200 | ₹3,500 | ₹3,100 | ₹3,000 | ₹2,900 | ₹3,300 | ₹2,800 | ₹2,900 | ₹3,100 | ₹2,750 |
| Interior Emulsion Paint (… | ₹420 | ₹440 | ₹410 | ₹400 | ₹395 | ₹430 | ₹390 | ₹395 | ₹420 | ₹385 |
Lowest price Highest price
About These Prices
- Prices are dealer-level rates for the specified city, updated weekly (every monday).
- Bulk orders (large quantities) typically get 3-10% discount.
- Prices exclude GST (which varies: 12% for cement, 18% for steel, etc.).
- Transportation costs are additional and vary by distance from dealer/factory.
- Always verify prices with 2-3 local dealers before purchasing.
Planning your construction budget?
Use our Cost Calculator to get a complete construction + interior estimate for your city.